In the compounds labeled MVRE and MVRE-HS (experimental surface-treated MVRE), 40% of N650 carbon black has been replaced with talc on an equal volumetric basis.
% N650 replaced 0 10 20 40 60 Die C tear, KN/m @ 23[degrees]C 16.7 19.1 28.9 26.5 28.6 @ 80[degrees]C 9.4 11.2 11.8 14.0 16.7 @ 121[degrees]C 6.6 8.6 9.5 10.2 10.4 Trouser tear, KN/m @ 23[degrees]C 3.2 3.9 4.7 8.9 4.9 @ 80[degrees]C 1.4 1.8 1.6 2.6 1.6 @ 121[degrees]C 0.9 0.9 1.2 1.6 1.1 Table 11--appendix--initial properties of EPDM cured with conventional sulfur, non-nitrosamine and EV systems Filler system CB MVRE MVRE-HS Cure system Conv.
The talcs referred to in this paper are Mistron Vapor R (MVR) or Mistron Vapor RE (MVRE).